LAM/COS100 – CONDITIONING SHAMPOO
Lamberti S.p.A
Preparation:
In the main vessel prepare phase A with gentle mixing until a clear viscous liquid is obtained and heat to 70-80°C. Add ingredients of phase C(C1,C2;C3), one by one, mixing well until a homogeneous product is obtained. In a side vessel disperse B2 into B1 and adjust pH to 7.00-8.00 and heat till to 50°C to better hydrate the polymer; add B into A; cool down the temperature of the main vessel and at 50°C add phase B and C4. Pre solubilize D2 into D3 and add it to the main batch.Notes:
Appearance : milky viscous liquid pH : approx 5.3 Viscosity (RVT Brookfield, 20 rpm, 25°C) : 20000 mPa·sDisclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
SNF, headquartered in Andrézieux, France, is a leading global producer of water-soluble polymers with primary manufacturing sites in France, the USA, and China. Over the last 40 years, SNF has developed expertise in polymer chemistries designed for specialty markets, such as personal care and cosmetics.
SNF’s Personal Care Division offers a...
Society of Cosmetic Chemists 78th Annual Scientific Meeting & Showcase
JW Marriot Los Angeles L.A. LIVE
11th - 13th December 2024
PCHi 2025
China Import and Export Fair Complex Guangzhou
19-21 February 2025