CLEAR MOISTURIZING SHAMPOO With Liponate® SB-50 NO. 1752
Vantage Specialty Ingredients, Inc.
Preparation:
1. Combine Sequence #1 ingredients in main vessel and heat to 75-80C with propeller mixing. 2. When Polyquaternium-10 is fully hydrated and clear, add Sequence #2 ingredients to main vessel and continue heating and mixing. 3. When batch temperature is 75-80C hold 10 minutes. 4. With continued mixing, slowly cool the batch. 5. When batch reaches 25C add Sequences #3, #4 and #5 with mixing, batch will thicken.Disclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
THERE IS NO SUBSTITUTE FOR PERFORMANCE
Whether you are formulating a standard personal care product or looking for the next texture innovation, Grant works ahead of the competition to deliver the formulation solutions you need. With an extensive portfolio of quality ingredients combined with our dedication to customer service, we deliver the...
in-cosmetics Korea 2025
COEX, Seoul
2nd - 4th July 2025
Breakthrough Science & Claims Testing - The SCS Annual Conference
Royal College of Surgeons of England, London
2 - 3 July