AGELESS CREAM With LIPOLIGHT® OAP/PVA NO. 1637
Vantage Specialty Ingredients, Inc.
Preparation:
PROCEDURE: 1. Mix Sequence #1 ingredients at 80?C with medium speed propeller stirring until dispersed. 2. Add Sequence #2 ingredients to main vessel with propeller mixing, heat to 80°C. 3. Heat Sequence #3 to 80°C, then add to Sequence #1 under propeller mixer. Mix for 15 minutes or until the emulsification is completed. 4. Remove from heat and add Sequence #4 to main vessel, batch will thicken slightly. 5. When batch is below 60°C add Sequence #5, and #6 with mixing and continue cooling. 6. Shutdown mixing when batch reaches 32°C.Notes:
SPECIFICATIONS: pH: 6.5 ± 0.2 Viscosity: TF at 3 rpm (Helipath:ON) = 458,900 cps ± 10% Stability: 30 days at 50°C (1) Lipo Chemicals, Inc. (9) Lubrizol (119) Ruger Chemical Co., Inc.Disclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
Capitalizing on more than 20 years of experience and great wealthy of Chinese plant resources (i.e Pineaceae, Mytaceae and Cupressaceae), Foreverest provides efficient, healthy, and eco-friendly products for global markets, including Rosin & Turpentine derivatives, Natural extract & synthetic aroma Chemicals. A thorough know-how of plant...
Society of Cosmetic Chemists 78th Annual Scientific Meeting & Showcase
JW Marriot Los Angeles L.A. LIVE
11th - 13th December 2024
PCHi 2025
China Import and Export Fair Complex Guangzhou
19-21 February 2025