Preparation:
Procedure Mix Phase A and B separately, without Carbopol and Keltrol, and heat up to 80°C. Disperse Keltrol and Carbopol in Phase A. Now blend Phase B without stirring to Phase A and homogenise. While homogenising add Phase C. Allow to cool down while stirring. Add Phase D at approx. 45°C and Phase E at room temperature. Properties pH: 5.8 Viscosity: 0.001 1/s - eta= 2257 Pas 5 1/s - eta= 9 Pas Rheology-Instrument: Haake RS1, sensor: PP 60/Ti, gap= 1.500 mm, T= 20°C, Controlled Stress Suppliers 1 Symrise GmbH & Co. KG 2 Cognis Dtl. GmbH 3 Degussa-Goldschmidt AG 4 Noveon 5 CP-KelcoDisclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Featured Supplier
We Ichimaru Pharcos a global company that contributes to the “health and beauty” of people all over the world by providing high-quality products through research/development and technology innovation in Japan.
After the establishment in 1959, ICHIMARU PHARCOS has become a global leader in Research and Development of natural active ingredients...
Upcoming Events
Cosmet’Agora
Espace Champerret – Paris
16th - 17th January 2024
PCHi
Shanghai World Expo Exhibition And Convention Center(SWEECC)
20th-22nd March 2024
in-cosmetics Global
Paris Expo Porte de Versailles
16th – 18th April 2024
Access the latest issue of Personal Care Magazine on your mobile device together with an archive of back issues.
Download the FREE Personal Care Magazine app from your device's App store