Jarchemtm Double Black Diamond Firming Clay Mask

Aurorium
Formula No. AK01046
Phase
Product
INCI Name
Supplier
Volume
A
Water
Water
59.86
Magnesium Aluminum Silicate
Magnesium Aluminum Silicate
Vanderbilt
4.50
B
Zemea™
Propanediol
Dupont Tate & Lyle Bioproducts
2.50
Glycerin
Glycerin
2.50
Xanthan Gum
Xanthan Gum
0.24
C
Jarxotic™ BLACK DIAMOND CLAY
Illite (and) Quartz (and) Kaolin
Jarchem
29.4
D
Euxyl™ K940
Phenoxyethanol (and) Benzyl Alcohol (and) Ethylhexylglycerin
Schülke
1.0

Preparation:

Procedure: 1. Add water to main vessel and heat to 65-70°C. Sprinkle in Magnesium Aluminum Silicate and mix for 15 minutes. 2. In a separate vessel, mix Phase B. 3. Remove Phase A from heat, and add Phase B to Phase A while mixing. 4. Add Phase C ingredients one at a time while mixing. 5. Add Phase D and mix.
Disclaimer

While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.

Latest Issues

in-cosmetics Latin America 2024

São Paulo, Brazil
25th - 26th September 2024

IFSCC 2024

Recanto das Cataratas Thermas Resort, Iguazu Falls, Brazil
14th - 17th October 2024