AFTER SUN RELIEF
Indena S.p.A
Preparation:
MANUFACTURING PROCEDURE Weight all ingredients of phase A), predisperse the polymer. Separately weight the components of phase B) and stir in water at 65°C. Add phase B) to phase A) while homomixing and stirring. Heat up to 70°C and add phase C) to phase B+A) while homomixing for 5 minutes. Slowly cool down and add phase D) at a temperature of 50°C. Prepare phase E) by predispersing Xilogel® in water at 55°C stirring for 30 minutes and then adding glycerine. Add phase E) to the emulsion. Slowly cool down and at 40°C add phase F) under homomixing.Notes:
CHARACTERISTICS: pH 5.5 +/- 0.5, T 20°C Density 9.95 +/- 0.05 g/ml Formulation developed in cooperation with ELLEGI BIOCOSMETICA, Assago, ItalyDisclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
Capitalizing on more than 20 years of experience and great wealthy of Chinese plant resources (i.e Pineaceae, Mytaceae and Cupressaceae), Foreverest provides efficient, healthy, and eco-friendly products for global markets, including Rosin & Turpentine derivatives, Natural extract & synthetic aroma Chemicals. A thorough know-how of plant...
NYSCC Suppliers' Day 2025
Javits Center, New York
3rd - 4th June 2025
17th Sun Protection Conference 2025
Royal College of Physicians, London
24 - 25 June 2025