Preparation:
Procedure • Sprinkle Carbopol® Ultrez 20 polymer onto the surface of water. Wait until the polymer has completely “wet out”. Start gentle agitation for 10 minutes. • Add PART A surfactants to the batch with gentle mixing. • Neutralize to pH 6.5 with sodium hydroxide solution while mixing. Heat to 65-70°C • Melt PART B in a separate vessel by heating to 65-70°C and then add to the batch. Mix until uniform and start cooling with agitation. • At 40°C, add PART C ingredients to the batch in order and mix until uniform.Notes:
Properties Appearance: White, shiny milky viscous liquid pH: 6.00-6.60 Viscosity: 5,000-7,000 mPa.s (Brookfield DV-II @ 20 rpm, #4 @ 21°C) Stability: Passed 3 months @ 45°C Passed 5 freeze/thaw cycles Suppliers 1 Noveon 2 GE Toshiba Silicones 3 RhodiaDisclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
Expertise at a Glance:
As part of Certified Group, Certified Laboratories is committed to delivering technical solutions and quality testing our customers can feel confident in – So The World Can Trust In What It Consumes™. Our network of FDA-registered, ISO 17025-accredited labs provides comprehensive testing services for cosmetics,...
IFSCC Congress 2025
Palais des Festivals, Cannes
15th - 18th September 2025
SEPAWA Congress 2025
ECC Estrel Center, Berlin
15-17th October 2025