Black Widow Mascara
Covation Bio PDO
Preparation:
1. Heat phase A to 85° C. 2. Add ingredients of phase A1 in given order and stir until completely dissolved. 3. Add and disperse A2 while stirring. 4. Add A3. 5. Homogenize phase A-A3 prior emulsification. 6. Heat phase B to 85° C. 7. Add phase A to phase B while stirring. Homogenize. 8. Add part C below 70° C. 9. Cool down to room temperature. Add ingredients of phase D below 40° CNotes:
• Appearance: black, viscous paste pH: 6,5-7,5 • Viscosity: Approx. 50000 mPas (Brookfield DVII: spindle 7, speed 10) • Stability: Stable for more than 3 months at 20° C, 40° C and 4° C.Disclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
THERE IS NO SUBSTITUTE FOR PERFORMANCE
Whether you are formulating a standard personal care product or looking for the next texture innovation, Grant works ahead of the competition to deliver the formulation solutions you need. With an extensive portfolio of quality ingredients combined with our dedication to customer service, we deliver the...
PCHi 2025
China Import and Export Fair Complex Guangzhou
19-21 February 2025
in-cosmetics Global 2025
RAI Amsterdam
8th - 10th April 2025