Volumizing Mascara With Non-Nano Carbon Black Composite KMA-041
Kobo Products
Preparation:
1. Heat Part 1 to 80°C with propeller mixing in auxiliary tank. 2. Add Part 2 ingredients at room temperature in main tank with propeller mixing. 3. Heat Part 2 to 80°C with homogenizer. 4. Add Part 1 to Part 2 with homogenizer at 80°C and continue to homogenize 15 minutes at 4000 rpm. 5. Switch to propeller mixing and cool batch to 50°C. 6. Add Part 3 at 50°C. 7. Add Part 4 at 50°C. 8. Cool to 25°C by mixing.Disclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
bitop - the global market leader and expert for biotechnological manufacturing & development of extremolytes Made in Germany. Extremolytes, natural stress protection molecules, are unique multifunctional ingredients with an outstanding efficacy. Ectoin® natural “the ultimate protection & repair” and Glycoin® natural “the cell energizer” are...
Cosmetorium
Palau de Congressos de Barcelona
23rd - 24th October 2024
in-cosmetics Asia 2024
BITEC, Bangkok, Thailand
5th - 7th November 2024