W/O Natural Ecocert Foundation With OD Dispersions KLF-080
Kobo Products
Preparation:
1. Combine Part 1 and mix until Magnesium Sulfate is dissolved. 2. Heat Part 2 until waxes are melted. 3. Homogenize Parts 2 and 3 together to 50°C. 4. Add Part 1 to Parts 2 and 3 once color is fully developed to room temperature. 5. Add Parts 4 and 5 while cooling and homogenizing slowly.Disclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
LipoTrue opens the door to further and more innovative science and technologies, overflowing with new concepts and novel active ingredients the dynamic and fast-changing cosmetic market. LipoTrue acts as a central R&D engine integrating cutting edge technology platforms in order to provide advanced active ingredients with proven and solid...
in-cosmetics Korea 2025
COEX, Seoul
2nd - 4th July 2025
Breakthrough Science & Claims Testing - The SCS Annual Conference
Royal College of Surgeons of England, London
2 - 3 July