This long-wear mascara contains Kobo's Carbon Black dispersion, WSJ10CB, for intense, deep, black color. Kobo's pigmentary dispersion, W60BBNFAP, is used in combination with WSJ10CB to provide the deep black shade and add film-forming properties. Kobo's resin composite, Koboguard® 5400 SQ, gives quick build up with a water-resistant film, and aids in long wear. SPC/BLACK NF-I2 hollow Microsphere complex with ITT adds building effect to the lashes.
Phase
Product
INCI Name
Supplier
Volume
A
Beeswax White SP 422
Beeswax
Strahl & Pitsch, Inc.
8.00
Ozokerite Wax White SP 1020
Ozokerite
Strahl & Pitsch, Inc.
5.00
Carnauba Wax SP 63
Copernicia Cerifera (Carnauba) Wax
Strahl & Pitsch, Inc.
3.00
Dermofat 4919
Stearic Acid
Alzo International Inc.
3.00
Microcrystalline Wax SP-89
Microcrystalline Wax
Strahl & Pitsch, Inc.
3.00
KOBOGUARD® 5400 SQ
Hydrogenated Polycyclopentadiene (And) Squalane
Kobo Products
2.00
Liposorb® SQO
Sorbitan Sesqioleate
Lipo Chemicals
1.00
Propyl Paraben NF
Propylparaben
0.10
B
Deionized Water
Water
33.15
W60BBNFAP
Iron Oxides (C.I. 77499) (And) Water (And) Ammonium Polyacrylate
Kobo Products
15.00
TEAlan 99%
TriethanolAmine
RITA Corp.
1.00
Natrosol® 250 HHR
Hydroxyethylcellulose
Hercules-Aqualon
0.30
Methyl Paraben NF
Methylparaben
0.20
C
Deionized Water
Water
6.00
Jeecide CAP-5
Phenoxyethanol (And) Caprylyl Glycol (And) Potassium Sorbate (And) Water (And) Hexylene Glycol
Jeen International
0.60
Germall® 115
Imidazolidinyl Urea
ISP
0.15
D
WSJ10CB
Black 2 (And) PEG-40 Hydrogenated Castor Oil (And) Water (And) Acrylates/Ethylhexyl Acrylate Copolymer (And) Aminomethyl Propanol (And) Sodium Dehydroacetate (And) Sodium Acrylate/Sodium Acryloyldimethyl Taurate Copolymer (And) Laureth-21
Kobo Products
15.00
SPC/BLACK NF-I2
Iron Oxides (C.I. 77499) (And) Ethylene/Methacrylate Copolymer (And) Isopropyl Titanium Triisostearate
Kobo Products
3.50

Preparation:

1. Heat Part 1 to 80°C in auxiliary tank. 2. Heat Part 2 to 80°C in main tank. 3. Add Part 1 to Part 2 in main tank with propeller and sweep agitation at 80°C. 4. Cool to 50°C. 5. Add Part 3 ingredients at 50°C. 6. Add Part 4 at 45°C. 7. Cool to 25-27°C.
Disclaimer

While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.

Latest Issues

Society of Cosmetic Chemists 78th Annual Scientific Meeting & Showcase

JW Marriot Los Angeles L.A. LIVE
11th - 13th December 2024

PCHi 2025

China Import and Export Fair Complex Guangzhou
19-21 February 2025